避免不锈钢铸件污染的方法: 1、高电压大电流密度冲击法。即就是在不锈钢铸件氧化初期就采用高压电击,使已被氧化的部分通过电击再连接成片。 2、表面打磨法。这个方法就是把打磨下来的铝磨填充已被氧化部分留下的缝隙,使产生的缝隙连接在一起,作为桥梁的作用。 3、表面喷丸法。这种方法就是用圆头锤子敲打缝隙,通过敲打使其闭合,可达到连成片的目的。 我们要根据不锈钢铸件被污染的程度选择相对应的对应方法。 Methods to avoid contamination of stainless steel castings: 1. High voltage and high current density impact method. That is to say, in the early stage of oxidation of stainless steel castings, high voltage shocks are used to make the oxidized parts connect by electric shock. 2. Surface grinding method. This method is to fill the gaps left by the oxidation part by grinding the aluminum mill, so that the crevice will be joined together as a bridge. 3. Surface shot peening. This method is to use a round head hammer to crack the gap, and to knock it off to achieve the goal of becoming a film. We should choose the corresponding method according to the degree of contamination of stainless steel castings.
版权所有保定宏晟隆精密铸造有限公司 网址:www.hslcasting.com.cn 保定网站制作:遨游网络
电话:0312-8928995 传真:0312-2115599 地址:保定南市区朱庄 推荐:不锈钢铸件,精密铸造,精密铸件,不锈钢铸件价格,精密铸件加工厂家
友链:光纤激光切割机 不锈钢铸件 过电压保护器 启闭机

保定网站建设及优化保定遨游网络公司